May I ask if the following questions, presented by a worried inspector, are legitimate and what would be the correct answers?
1) - AWS D1.1-2008-Fig 4.27-
6GR Test specimen used to qualify 6GR Welder.
AWS Table 4.10 - limits the qualification with Note "d"
thus basically he is not qualified to weld pipe where internal access is not possible.
Why this limitation required/included?
2) - ASME Sect IX does not have any provisions for 6GR Qualification as a 6G welder qualified to weld all position except for QW-303.3 - which refer to 'special position'.
Can 1GR / 6GR welder test position be confirmed as "Special Joint"?
Thanks, regards
1) - AWS D1.1-2008-Fig 4.27-
6GR Test specimen used to qualify 6GR Welder.
AWS Table 4.10 - limits the qualification with Note "d"
thus basically he is not qualified to weld pipe where internal access is not possible.
Why this limitation required/included?
2) - ASME Sect IX does not have any provisions for 6GR Qualification as a 6G welder qualified to weld all position except for QW-303.3 - which refer to 'special position'.
Can 1GR / 6GR welder test position be confirmed as "Special Joint"?