AWS D1.1 2015 new Clause 9.
Previous versions of D1.1 Table 4.2 (2. Test on Pipe or Tubing). Previous wording was "Nominal Plate, Pipe or Tube Wall Thickness Qualified, in". The new 2015 version reads "Nominal Pipe or Tube Wall Thickness Qualified, in". The word Plate is missing, is this an oversight and is Plate still qualified when a pipe coupon is used?
Thanks
wp23
Previous versions of D1.1 Table 4.2 (2. Test on Pipe or Tubing). Previous wording was "Nominal Plate, Pipe or Tube Wall Thickness Qualified, in". The new 2015 version reads "Nominal Pipe or Tube Wall Thickness Qualified, in". The word Plate is missing, is this an oversight and is Plate still qualified when a pipe coupon is used?