Dear Friends
Pls provide best possible clarification/definition asap
Code- AWS D1.1 Year 2010
The omission, but no inclusion, of backing or backgouging
1st i prfer to break it up
1- Omission of backing or backgouging- If PQR qualified with backing ( backing weld/backing strip/metallic strip) or backgouging, then this PQR also can be used for single-sided production welding. But is it can be used to do back-weld on internal side where accessible( root side-no backing/backgouging done ) for weld repair touch-ups?
Thanks
Pls provide best possible clarification/definition asap
Code- AWS D1.1 Year 2010
The omission, but no inclusion, of backing or backgouging
1st i prfer to break it up
1- Omission of backing or backgouging- If PQR qualified with backing ( backing weld/backing strip/metallic strip) or backgouging, then this PQR also can be used for single-sided production welding. But is it can be used to do back-weld on internal side where accessible( root side-no backing/backgouging done ) for weld repair touch-ups?
Thanks