Sep 6, 2002 #1 PAN Mechanical Apr 25, 2001 549 0 0 SG For alloy 400, the user's requiremnet is flat bar (12 mm. thickness, 90 mm. width). What's the suitable reference ASTM B127 or B164?
For alloy 400, the user's requiremnet is flat bar (12 mm. thickness, 90 mm. width). What's the suitable reference ASTM B127 or B164?
Sep 6, 2002 1 #2 TVP Materials Apr 12, 2002 4,592 0 0 US ASTM B 164 defines a bar as being at least 3.2 mm thick and up to 254 mm wide, so you should order this material according to ASTM B 164. Upvote 0 Downvote