timmckee
Mechanical
- Oct 19, 2005
- 20
I'm confused over the allowable surface porosity for girth welds in all fluid services.
Table 341.3.2A states that the extent of imperfection allowed is zero, however it also refers to Note 5 (These imperfections are evaluated for welds less than or equal to 3/16" in nominal thickness).
Does this mean that surface porosity is allowed for welds over 3/16" and if so what is the acceptance criteria?
Table 341.3.2A states that the extent of imperfection allowed is zero, however it also refers to Note 5 (These imperfections are evaluated for welds less than or equal to 3/16" in nominal thickness).
Does this mean that surface porosity is allowed for welds over 3/16" and if so what is the acceptance criteria?