I am reviewing a specification for a gas pipeline (material API 5L PSL2) with a minimum temperature of -50F. According to B31.8, this triggers Annex G of API 5L. I am really struggling to sort the actual requirements of CVN and/or DWT testing.
- My understanding is that shear area is calculated from DWT and absorbed energy from the charpy (CVN) test. Is that correct?
- If the above is true, how is the shear area requirement (85%) of G.3.1 determined for line sizes </=20 in since the DWT test is apparently not applicable in that range?
- What is meant by a full-size test piece? My understanding is that CVN tests are performed on 10mmx10mmx55mm samples. Is this applicable to DWT?
- I assume the greater value of API 5L Table 8 or Annex G should be used (since we specifying PSL2 pipe) for minimum CVN energy.
Thanks in advance
- My understanding is that shear area is calculated from DWT and absorbed energy from the charpy (CVN) test. Is that correct?
- If the above is true, how is the shear area requirement (85%) of G.3.1 determined for line sizes </=20 in since the DWT test is apparently not applicable in that range?
- What is meant by a full-size test piece? My understanding is that CVN tests are performed on 10mmx10mmx55mm samples. Is this applicable to DWT?
- I assume the greater value of API 5L Table 8 or Annex G should be used (since we specifying PSL2 pipe) for minimum CVN energy.
Thanks in advance