Section 826.2(b) in B31.8 (2003) contains the term "field butt welds" which, to me, implies just that...butt welds that are made in the field (not a shop).
I'm working a design that meets the hoop stress criteria of 826.2 but the welding will be performed in a shop environment. For lack of equivalent guidance for "shop butt welds" I'm compelled to use what's given despite the "field" referene.
Has anyone ran this trap before and with what results?
I'm working a design that meets the hoop stress criteria of 826.2 but the welding will be performed in a shop environment. For lack of equivalent guidance for "shop butt welds" I'm compelled to use what's given despite the "field" referene.