i am searching for basic allowable stresses for the following material which is not listed in B31.3:

SB-705 N06625 60Ni - 22Cr - 9Mo - 3.5Cb Wld. Pipe Annealed

in the -20 to 1000 degF range

many thanks.
 
B-705 N06625 is listed in Table A-1 of ASME B31.3.

SB is ASME spec (same material) listed under the Boiler Pressure Vessel Code.

For B31.3 piping you can use the allowable stresses of the B-705 material in B31.3.
 