Hello everyone,
We have to overhaul an old machine, its a marine loading arm manufactured in 1980. On top of column there is mounted a big bearing with 3 ball races. The ball races show flase brinneling marks. The bearing is manufactured in such a way that there are 3 semicicular tracks machined in the steel body, and then in each of the track there is mounted a ball race. This ball race can be removed and replaced, but since the bearing is from 1980 the manufacturer is out of business and its a bit difficult to find the replacement.
In these conditions, our foreman is proposing cold pressing of ball race to remove the false brinneling marks. He is proposing to press a ball against the ball race mounted in the track, and to rotate the ball a few times.
But to me this does not seem like a proper solution, I am thinking to anneal the ball races first and then check further steps to be done. I am trying to find some literature regarding this.
I dont know which appraoch is right, or maybe both approaches are wrong. Any help will be much appreciated.
Thanks.
We have to overhaul an old machine, its a marine loading arm manufactured in 1980. On top of column there is mounted a big bearing with 3 ball races. The ball races show flase brinneling marks. The bearing is manufactured in such a way that there are 3 semicicular tracks machined in the steel body, and then in each of the track there is mounted a ball race. This ball race can be removed and replaced, but since the bearing is from 1980 the manufacturer is out of business and its a bit difficult to find the replacement.
In these conditions, our foreman is proposing cold pressing of ball race to remove the false brinneling marks. He is proposing to press a ball against the ball race mounted in the track, and to rotate the ball a few times.
But to me this does not seem like a proper solution, I am thinking to anneal the ball races first and then check further steps to be done. I am trying to find some literature regarding this.
I dont know which appraoch is right, or maybe both approaches are wrong. Any help will be much appreciated.
Thanks.