Jan 20, 2023 #1 siridi Petroleum Jun 9, 2020 6 0 0 DZ Dear all, which method is best and required for pitting corrosion between A923 method c and G48 method A. regards.
Dear all, which method is best and required for pitting corrosion between A923 method c and G48 method A. regards.
Jan 20, 2023 1 #2 SJones Petroleum Apr 22, 2001 3,890 1 38 GB A923 Test Method C is more defined for application to duplex and superduplex stainless steels. G48 testing in accordance with ISO 17781 is the current international standard for DSS/SDSS materials. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
A923 Test Method C is more defined for application to duplex and superduplex stainless steels. G48 testing in accordance with ISO 17781 is the current international standard for DSS/SDSS materials. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer.