I saw some other threads on this issue, but they were several years old and did not seem to match my situation. We're on a deep well in a rural area in the piedmont of western North Carolina. My well is deep, 500'+ in granite. We do see a blue color in the bath tub and some staining on the shower grout. Our water is somewhat aggressive with a pH of 6.5, alkalinity of 14mg/l and hardness of 8mg/l. BUT, we have pvc piping in the well, pvc from the well to the house, and PEX throughout the home. I took a sample in the bathroom to see if the cu concentration was high enough to cause the color and the sample tested at 1.08mg/l. I find it hard to believe that the color could be coming from brass plumbing fittings. Since the concentrations are not high enough to be a heath concern I'm inclined to let it go, but my wife is still concerned. Am I missing something or should I be concerned? Thanks for any advice you may have.