Hi,
the bolts material specified for assembly of WET SOUR process piping (non exposed to fluid) was SA 193 B7M. Due to a mistake in our material take-off software, SA 194 Gr L7 was specified for nuts instead of SA 194 Gr 2HM (22HRC). This material is qualified under a hardness (24-38 HRC). Because of this material is not in contact with fluid, it is in compliance with NACE MR0175 but we are not confident about a excessive wear may happen in the bolt material due to the difference in hardness.
Please advise.
Peter
the bolts material specified for assembly of WET SOUR process piping (non exposed to fluid) was SA 193 B7M. Due to a mistake in our material take-off software, SA 194 Gr L7 was specified for nuts instead of SA 194 Gr 2HM (22HRC). This material is qualified under a hardness (24-38 HRC). Because of this material is not in contact with fluid, it is in compliance with NACE MR0175 but we are not confident about a excessive wear may happen in the bolt material due to the difference in hardness.
Please advise.
Peter