I want to tight the bolts of for example one 20 inch flange.
I know the bolt size and bolt material.
I have calculated the yielding strenght for bolt material.
Now what should I do?
Find out what gasket you are using and then ask the manufacturer of the gasket what bolt material and torque you should use. Or as mentioned above, get PCC-1, read it so you can figure it out.