I’m involved in a project where we need to bond plastics like FFKM (Kalrez) & PCTFE (Kel-f) in a device that in service will see saturated solvent atmosphere ( DMSO, Acetone, Acetonitrile, toluene, dichloromethane among the most significant) to 100°C, or with less aggressive environment will see close to 250°C.
Previous research by a colleague (including some testing) for a slightly different application suggests that Torr-Seal has the best resistance to the solvents (out of adhesives he looked at) but possibly doesn’t bond the FFKM & PCTFE materials well and has a temperature limit of 120°C.
We typically use Chemgrip for bonding plastics like these but it does not stand up well to the solvents. We typically use MASTERBOND 10HT for high temp, but again not great with some chemicals.
I’m doing some digging and came across MasterBond EP45HT which claims solvent compatibility & good temperature performance does anyone have any experience using this (I’ll try contacting them but apparently my colleague had trouble getting information from them previously and had concerns about their claims for some other formulations so I thought I’d see if anyone here has used it.)
In my colleagues research he also came across D.E.N. 438 Epoxy Novolac Resin but didn’t get as far as testing it, and had concerns about it being tricky to work with in production.
A related formula D.E.N. 431 looks even better.
Another company they found was Arcor especially EE-101
Quick Google search turned up Loctite 325
If any one has any experience with these or suggestions of alternatives I’d appreciate it.
I’m involved in a project where we need to bond plastics like FFKM (Kalrez) & PCTFE (Kel-f) in a device that in service will see saturated solvent atmosphere ( DMSO, Acetone, Acetonitrile, toluene, dichloromethane among the most significant) to 100°C, or with less aggressive environment will see close to 250°C.
Previous research by a colleague (including some testing) for a slightly different application suggests that Torr-Seal has the best resistance to the solvents (out of adhesives he looked at) but possibly doesn’t bond the FFKM & PCTFE materials well and has a temperature limit of 120°C.
We typically use Chemgrip for bonding plastics like these but it does not stand up well to the solvents. We typically use MASTERBOND 10HT for high temp, but again not great with some chemicals.
I’m doing some digging and came across MasterBond EP45HT which claims solvent compatibility & good temperature performance does anyone have any experience using this (I’ll try contacting them but apparently my colleague had trouble getting information from them previously and had concerns about their claims for some other formulations so I thought I’d see if anyone here has used it.)
In my colleagues research he also came across D.E.N. 438 Epoxy Novolac Resin but didn’t get as far as testing it, and had concerns about it being tricky to work with in production.
A related formula D.E.N. 431 looks even better.
Another company they found was Arcor especially EE-101
Quick Google search turned up Loctite 325
If any one has any experience with these or suggestions of alternatives I’d appreciate it.