Bulb Flats - weld bevel

Status
Not open for further replies.

Nomismum

Petroleum
Aug 24, 2008
8
FR

We are having to replace a section of bulb flat and I wondered if there was a specific weld bevel required. I have looked in "No.47 Shipbuilding and Repair Quality Standard" but although the order of welds and some weld bevel examples are given the weld bevels all refer to flat plates and not bulb flats.

Which specification should I be referring to.