Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations pierreick on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

butt joint welding (dissimilar thicknesses) with impact requirement

Status
Not open for further replies.

FernandoL

Industrial
Jun 29, 2016
9
Hi, colleagues,

May I qualify a WPS according to AWS D1.1 for the following joint: [butt joint 1/2V bevel, T1=10mm, T2=30mm CVN required] through a test piece composed of plates of dissimilar thicknesses (the same thicknesses as the production joint above)?

or should I conduct the elaboration of 2 PQR, each one with equal thickness plates, one with T=10mm and the other with T=30mm thick plate, and at the end issue WPS based on the two PQR mentioned above?

despite my best efforts, I didn't find any reference to this situation in AWS D1.1.

Any help will be very useful.



 
Status
Not open for further replies.

Part and Inventory Search

Sponsor