Feb 17, 2006 #1 dungun Mechanical Dec 30, 2005 39 MY Hi Construction of ASME Viii Div i spherical tank. I have joints thickness 40mm with double groove. Problem to control the shringkage, in the codes any permission for buttering?.
Hi Construction of ASME Viii Div i spherical tank. I have joints thickness 40mm with double groove. Problem to control the shringkage, in the codes any permission for buttering?.
Feb 17, 2006 #2 metengr Materials Oct 2, 2003 15,478 US Yes. Buttering is just a weld technique that typically becomes part of the finished groove weld deposit. Upvote 0 Downvote
Yes. Buttering is just a weld technique that typically becomes part of the finished groove weld deposit.
Feb 17, 2006 #3 deanc Specifier/Regulator Sep 18, 2002 855 US See UW-42 for buttering. See UW-35 for shrink. Upvote 0 Downvote