CA6NM 2

Status
Not open for further replies.

lidbasky

Materials
Apr 19, 2011
39
Hi,
Could anybody help me to find CA6NM steel TTT diagram?
I look in Heat treaters guide and I cant find it?
 
Replies continue below

Recommended for you

Try F6NM (forged): there will be some differences, but there are also differences between heats of CA6NM. It has very good hardenability, but in my opinion, a complex response to HT. (MAY respond to double tempering, cryogenic cooling , etc).
 

You can see the ttt curve. Being a soft martensitic steel,fast air cooling followed by double tempering is the normal practice.

_____________________________________
"The richer we have become materially, the poorer we have become morally and spiritually." Martin Luther King Jr
 
CA-6NM has good hardenability to essentially unlimited thickness, but it is sensitive to compositional differences: the final hardness is extremely sensitive to carbon content, and nickel is an important actor in depressing the Ms temperature. I searched my documents but could not find either a TTT or CCT diagram.

A lot of the general literature makes the mistake of lumping it in with other 400-based martensitics when talking about heat treatment, welding, and PWHT of CA-6NM. It is a unique alloy in many respects.
 
We tempered our casting in 680 C. Is the retain austenite harmful for mechanical properties?
I need TTT diagram for CA6NM Cast steel.
 
Brinstoner, yes! Thats what I was trying to say, more data in ASTM ATP 756,and it is the only alloy that MR 01-75 allows non-standard hardness conversion. Lidbasky; you may need a metallurgist.
 
I am metallurgist but I need TTT diagram for finding Ms & Mf .....
 
Is retain austenite in CA6NM harmful when part working in high temprature?
 
No. The problem is upon cooling from high service temperature to lower temperature and the transformation to unptempered (new)martensite.
 
Let me revise what I stated moments ago... if the component is continually operating where creep deformation is a concern, retained austenite would certainly be a problem as well as elevated temperature strength properties.
 
Thank you for your reply Metengr. I get the diagram that Arunmrao give its link, but its carbon content is very low about 0.02%.I need some reliable document about TTT diagram to disscuse with my purchaser. I studied Atlas of TTT diagrams but i couldnt find it.
 
Status