Hi,
I have to check suitability of the selected beam. The problem is that I'm working with aluminum so I can't find a table that has allowable moments, deflection and shear, which means I have to calculate them myself. (Unless anyone knows of a table of allowable moments and shear?) The beams are simply supported on each end.
I have 3 types of beams (SI units):
1. 100x50x6 Channel
2. 100x10 Solid Rectangle
3. 100x75x6 Hollow Section
They are 6061 T-6 Aluminum which has a 275 MPa yield strength, ultimate 310 MPa and Elongation % on 2" of 12 if that is needed.
The factored loading and lengths are:
1. 6.32 KN/m 2.78m
3. 6.82 KN/m 2.89m
4. 6.13 kN/m 2.21m
I have to check suitability of the selected beam. The problem is that I'm working with aluminum so I can't find a table that has allowable moments, deflection and shear, which means I have to calculate them myself. (Unless anyone knows of a table of allowable moments and shear?) The beams are simply supported on each end.
I have 3 types of beams (SI units):
1. 100x50x6 Channel
2. 100x10 Solid Rectangle
3. 100x75x6 Hollow Section
They are 6061 T-6 Aluminum which has a 275 MPa yield strength, ultimate 310 MPa and Elongation % on 2" of 12 if that is needed.
The factored loading and lengths are:
1. 6.32 KN/m 2.78m
3. 6.82 KN/m 2.89m
4. 6.13 kN/m 2.21m