bydublin
Chemical
- Dec 20, 2007
- 6
Hi,
Can anybody help on the calculation for the wall thickness of a storage tank 98"OD x 216"straight side? The SS304L tank is vertical with cone top and flat bottom at atmospheric temperature and pressure to hold 67% HNO3 (1.41kg/l or 11.7 lb/gal). We had a proposal with 10gauge SS304L for this tank. But not sure if it is safe for tank with this height. Highly appreciate your advice.
Thank you!
bydublin
Can anybody help on the calculation for the wall thickness of a storage tank 98"OD x 216"straight side? The SS304L tank is vertical with cone top and flat bottom at atmospheric temperature and pressure to hold 67% HNO3 (1.41kg/l or 11.7 lb/gal). We had a proposal with 10gauge SS304L for this tank. But not sure if it is safe for tank with this height. Highly appreciate your advice.
Thank you!
bydublin