Hi,
I need confirmation that ¿is possible replace ASTM A194 Gr.4 nuts by Gr.7?
The ASTM A-194 in paragraph 7.2 say "Grade 7 may be substituted for Grade 4. When such substitution is made, the nuts shall be marked as Grade 7", but I'm not know if this change is possible in opposite case.

Thanks for you answer.

Marcos Díaz.
 
"substitute" = "replace"

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Which edition of the ASTM specification has this statement? 7.2 in the 00 Edition refers to proof load test.
 
Hi metengr,

The standard available in my company is 2015.

I have reviewed the norm again and the table 1 of chemical composition, indicates that for the Gr.4 applies his G-Note. The note G says exactly:

"Grade 4 is expected to be withdrawn within approximately 2 years. Grade 7 is an acceptable substitute for Grade 4. See 7.2"

This clarifies this issue and definitely the interpretation is that grade 7 can replace grade 4.

Tnahk you all.[wink]
 