Jan 11, 2011 #1 rauval Mechanical Jun 2, 2009 7 0 0 US Under what conditions can foreign materials be used as ASME materials? Is there a procedure to certify European steels as ASME materials?
Under what conditions can foreign materials be used as ASME materials? Is there a procedure to certify European steels as ASME materials?
Jan 11, 2011 #2 metengr Materials Oct 2, 2003 15,478 0 0 US Yes. Read ASME B&PV Code, Section II, Introduction GUIDELINE ON THE APPROVAL OF NEW MATERIALS UNDER THE ASME BOILER AND PRESSURE VESSEL CODE Upvote 0 Downvote
Yes. Read ASME B&PV Code, Section II, Introduction GUIDELINE ON THE APPROVAL OF NEW MATERIALS UNDER THE ASME BOILER AND PRESSURE VESSEL CODE
Jan 11, 2011 1 #3 trottiey Nuclear Jul 8, 2010 237 0 0 CA That would be Section II, Appendix 5. That's one option if you plan on doing this a lot. Or you can look at UG-10, or its equivalent in other codes of construction, for ad hoc cases. Upvote 0 Downvote
That would be Section II, Appendix 5. That's one option if you plan on doing this a lot. Or you can look at UG-10, or its equivalent in other codes of construction, for ad hoc cases.
Jan 11, 2011 #4 trottiey Nuclear Jul 8, 2010 237 0 0 CA Check out page 4 of the attached ASME newsletter: http://files.asme.org/asmeorg/Codes/CertifAccred/Accreditation/1030.pdf Upvote 0 Downvote
Check out page 4 of the attached ASME newsletter: http://files.asme.org/asmeorg/Codes/CertifAccred/Accreditation/1030.pdf