Mar 7, 2008 #1 heloman29 Aerospace Oct 25, 2007 21 0 0 US I'm trying to figure out what BS (British standard) L65 Aluminum converts to. Possibly 2024 T??? Thanks for the help!!
I'm trying to figure out what BS (British standard) L65 Aluminum converts to. Possibly 2024 T??? Thanks for the help!!
Mar 7, 2008 #2 TVP Materials Apr 12, 2002 4,592 0 0 US Take a look at this thread. The CASTI Red Book would be a good place for authoritative conversions of BS aluminium grades to ASTM, SAE, etc. thread2-178465 Upvote 0 Downvote
Take a look at this thread. The CASTI Red Book would be a good place for authoritative conversions of BS aluminium grades to ASTM, SAE, etc. thread2-178465
Mar 7, 2008 #3 PBroad Mining Mar 27, 2002 113 0 0 CA Try Metal Resource directory, if it's not there there should be a link http://www.metalresourcesdirectory.com/top_rated.php Upvote 0 Downvote
Try Metal Resource directory, if it's not there there should be a link http://www.metalresourcesdirectory.com/top_rated.php
Mar 10, 2008 #4 geoffthehammer Mechanical Jan 28, 2005 77 0 0 GB L65 was replaced by 2L77 and L168 2L77 is 2014A Forging stock and forgings L168 is 2014A Bars and sections Hope this helps Upvote 0 Downvote
L65 was replaced by 2L77 and L168 2L77 is 2014A Forging stock and forgings L168 is 2014A Bars and sections Hope this helps