REQMNT NEEDS ASTM A148 Gr 90/60 CAST PLT 25mm THK - CAN EQUIVALENT STRUCTURAL PLT GRADE EN10113 S420/ S460NL1 (OR EQUAL)BE USED INSTEAD? OR WILL CAST PLT HAVE PROPERTIES THE STRUCTURAL GRADE CAN'T EMULATE OR ACHIEVE?
 
Replies continue below

Recommended for you

It is up to your client or customer. In most cases, a casting provides minimal machining and fabrication in comparison to wrought plate. Also, wrought plate will exhibit directionality in mechanical properties in comparison to a cast product.
 