Feb 8, 2005 #1 Shofa Mechanical Jun 18, 2002 21 0 0 SA Could you please tell me which better and why: a- Using CS for the bottom of CS storage tank with CP. OR B- Use SS for the bottom of CS storage tank without CP. regards,
Could you please tell me which better and why: a- Using CS for the bottom of CS storage tank with CP. OR B- Use SS for the bottom of CS storage tank without CP. regards,
Feb 9, 2005 1 #2 mshimko Materials Oct 27, 2004 364 0 0 US More information is needed: 1. What is being stored in the tanks? 2. Will the CS be painted or unpainted? 3. Will the SS be painted or unpainted? Upvote 0 Downvote
More information is needed: 1. What is being stored in the tanks? 2. Will the CS be painted or unpainted? 3. Will the SS be painted or unpainted?
Feb 10, 2005 #3 PAN Mechanical Apr 25, 2001 549 0 0 SG I understand that galvanic corrosion will be a problem in your option B (SS bottom, CS shell). The additional information as mshimko's comment is also necessary. Upvote 0 Downvote
I understand that galvanic corrosion will be a problem in your option B (SS bottom, CS shell). The additional information as mshimko's comment is also necessary.