Hi everybody,
I have the PQR following ASME IX with Process: GTAW, CVN at -40 Degree,Filler Metal: ER 316, Diameter: 2.4 mm, Range amper rate: 69 to 82 A, Votage: 9 to 13 V, Heat input: 0.98 to 2.5 J.
Now, i want to write one WPS for weld joint socket weld (fillet weld)with wall thickness is 1.5 mm, OD is 1/2 inch, not require CVN test, So i need to reduce range amper: 45 to 50 A and diameter filler is 1.6 mm.
Summary, can i use PQR above to write this wps.
 
Replies continue below

Recommended for you

Since you have the original PQR, open Section IX and review the WPS essential variables for the GTAW process in QW-256. If essential variables listed in QW-256 are not changed by writing a new WPS, you can use the new WPS under the supporting PQR.
 
Assuming that you don't have a copy of ASME IX, you can revise the existing WPS or write a new WPS using the existing supporting PQR. And if you don't have a copy, get one!
 