gayaz
Mechanical
- Aug 7, 2001
- 18
I designed a shell of 127 ID and 60 in length in advance pressure vessel software. the software says that the result is questionable and says charpy test is required?. Can any one explain why charpy test is required? I am doing Full RT, 100% weld efficiency.
thanks