Timeyin
Mechanical
- Sep 5, 2013
- 17
Hi All,
I'm faced with a little issue and i'm really hoping you guys will enlighten me.
I've designed and routed an underground water pipe system (fire ring main) for a gas handling facility. A 10" header at 600mm from top of pipe to the finished ground level, distributes water to all the branch out.
My main issue here is with regards protective coating for the section of the pipe that will be buried.
I'm conversant with coating code LC4-N which involves the use of Epoxy Primer 2 coats of epoxy and a total minimum NDFT of 500μm. But my client is insisting that my specified coating system (LC4-N)be used in combination with cathodic protection. Quite frankly i'm not too familiar with cathodic protection systems and would try to avoid it as much as possible.
My question is - Is my specified coating system adequate to protect the pipe from corrosion?
Is my client right?
If yes, Which code/standard validates my client's point?
When is it absolutely compulsory to cathodically protect a buried pipe?
Which code/standard can point me to the right path.
I look forward to hearing from you guys.
I'm faced with a little issue and i'm really hoping you guys will enlighten me.
I've designed and routed an underground water pipe system (fire ring main) for a gas handling facility. A 10" header at 600mm from top of pipe to the finished ground level, distributes water to all the branch out.
My main issue here is with regards protective coating for the section of the pipe that will be buried.
I'm conversant with coating code LC4-N which involves the use of Epoxy Primer 2 coats of epoxy and a total minimum NDFT of 500μm. But my client is insisting that my specified coating system (LC4-N)be used in combination with cathodic protection. Quite frankly i'm not too familiar with cathodic protection systems and would try to avoid it as much as possible.
My question is - Is my specified coating system adequate to protect the pipe from corrosion?
Is my client right?
If yes, Which code/standard validates my client's point?
When is it absolutely compulsory to cathodically protect a buried pipe?
Which code/standard can point me to the right path.
I look forward to hearing from you guys.