Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

cold forming of shell plates

Status
Not open for further replies.

fazel2

Materials
Nov 21, 2008
16
IR
Is it acceptable to form a 100mm thckness shell plate of a HP drum by cold forming(rolling) process?
Design code is ASME SecI
 
Replies continue below

Recommended for you

Yes. There are manufacturers which possess plate rolls capable cold forming 100 mm plate. Also more than likely the Drum will be subject to PWHT in a furnace by the manufacturer. This will stress relieve the cold forming stresses in the shell as well as the Code mandated stress relief of the welds.

 
In cold forming ,some grain deformation will happen. Does this require normalizing process or just stress relieving is enough?
 