I recently had 6061 aluminum braces (1/8”thick) welded onto 6061 aluminum carts. I am not sure whether these were welded with TIG or MIG processes. However, the welded
areas has excessive spatter and the carts are now distorted and misaligned. What, if any, pre heat or post heat is required when welding aluminum with TIG or MIG? Can I cold or hot work these carts to correct for misalignment, and what are the recommended temperatures?
 
Replies continue below

Recommended for you

If there is spatter around the weld it will not have been TIG welded as this is a 'clean' method of welding.
 

if there is a spatter it is because of mig welding and you can do cold to some extent, it is better to do some preheating
 