Hi,

Is someone able to explain the Sec IX QW 200.4 (B)to me...

Thanks
 
Replies continue below

Recommended for you

The short of it is that it permits you to use multiple PQR's to support a WPS, if the PQR was qualified on 1/2" material or greater. This is most useful in creating dual-process procedures (such as GTAW root pass with SMAW fill), and for increasing thickness qualified.
 