emilywalters
Civil/Environmental
- Oct 15, 2012
- 13
BS EN 1993-5:2007 Clause 5.5.2 (7) States:
For sheet piles used as secondary elements, further verification may be omitted if all the following conditions are met:
- wall thickness of the sheet piles: >or= 10mm;
- ...
For design of a harbour wall, does anyone know if this requires the designer to select a section with an uncorroded thickness >or= 10mm or whether the corroded section must be >or= 10mm. A reference for justification would be great.
Many Thanks!
For sheet piles used as secondary elements, further verification may be omitted if all the following conditions are met:
- wall thickness of the sheet piles: >or= 10mm;
- ...
For design of a harbour wall, does anyone know if this requires the designer to select a section with an uncorroded thickness >or= 10mm or whether the corroded section must be >or= 10mm. A reference for justification would be great.
Many Thanks!