Jul 19, 2005 #1 EngForm78 Mechanical May 6, 2005 29 0 0 US WHat are the common materials for heating elements. WHat are the main factors, I would guess resistance and melting temp, but I am not sure.
WHat are the common materials for heating elements. WHat are the main factors, I would guess resistance and melting temp, but I am not sure.
Jul 19, 2005 #2 IRstuff Aerospace Jun 3, 2002 44,351 4 38 US Nichrome is used in lots of heating applications TTFN Upvote 0 Downvote