We will need to increase the reinforcing area of some nozzles in an existing Pressure Vessel due to some modifications in the Operating Conditions. These nozzles are already reinforced with Pads nowadays. The easiest way would be welding another Pad over the existing one. Does anyone have experience on doing this? Is there anything in ASME Code Sec. VIII that doesn´t permit this type of solution?