I'm trying to find out general location and shapes of cracks in the foundation due to freeze/thaw, corrosion or even carbonation.
The cracks that I'm seeing is a shallow footing with cracking all around at around 3~4" above grade. It seems like cracks/separation is happening at concrete covers.
I don't see heavy leeching of rebar corrosion. Any ideas? I've attached a sketch in an attempt to illustrate this.
The cracks that I'm seeing is a shallow footing with cracking all around at around 3~4" above grade. It seems like cracks/separation is happening at concrete covers.
I don't see heavy leeching of rebar corrosion. Any ideas? I've attached a sketch in an attempt to illustrate this.