Sep 30, 2023 #1 haynewp Structural Dec 13, 2000 2,297 0 36 US I’m looking for non-shrink product recommendations to fully fill some existing horizontal core holes in a concrete column that are 3” dia x 2 feet long. I need min 5000 psi but it also needs to be flowable to fully fill the holes. Thanks
I’m looking for non-shrink product recommendations to fully fill some existing horizontal core holes in a concrete column that are 3” dia x 2 feet long. I need min 5000 psi but it also needs to be flowable to fully fill the holes. Thanks
Sep 30, 2023 1 #2 bridgebuster New member Jun 27, 1999 3,962 0 0 US Try SikaGrout 212. I've used it for filling pockets in prestressed concrete box beams. Upvote 0 Downvote