Sep 6, 2013 #1 Aliq298 Industrial Dec 29, 2011 16 0 0 MY Dear all expert, I need confirmation..if qualified wps is double bevel, can we use it for single bevel.. Regards,
Dear all expert, I need confirmation..if qualified wps is double bevel, can we use it for single bevel.. Regards,
Oct 5, 2013 #2 pandithan Mechanical May 20, 2001 101 0 0 IN CJP GROOVE WELD QUALIFIES ANY GROOVE WELD Upvote 0 Downvote