I am looking to your kind consultation of pressure test requirements which are written in BS 1868 (Chapter-36 Production pressure testing) as quoted below:
Quote:
All valves shall be pressure tested by the manufacturer before despatch in accordance with BS 6755-1, as below:
a) hydrostatic shell test;
b) hydrostatic seat test;
c) hydrostatic seat test at 25 % of the seat test pressure required for test b).
Unquote:
As I am not experienced in testing of valves, could you kindly advise if c) above requires a pressure test at 25% of pressure level of item b) above and why item c) is required whereas it could be covered by item b), in term of test pressure level?
Thanks a lot.
Quote:
All valves shall be pressure tested by the manufacturer before despatch in accordance with BS 6755-1, as below:
a) hydrostatic shell test;
b) hydrostatic seat test;
c) hydrostatic seat test at 25 % of the seat test pressure required for test b).
Unquote:
As I am not experienced in testing of valves, could you kindly advise if c) above requires a pressure test at 25% of pressure level of item b) above and why item c) is required whereas it could be covered by item b), in term of test pressure level?
Thanks a lot.