I'm trying to replace/modify a series of valves that reduces pressure from 1600 psi to 400 psi. There is currently one PRV along with an isolation valve in series. Both get steam/condesate cut in a matter of months. These valves are cycled approx. twice a day.
Will replacing the isolation valve with another PRV help the situation? This would allow two pressure drops across two valves from 1600 to 400 psi.
Also, does steam cut valves when they are cycled or condesate or both?
Thanks for the input.
Will replacing the isolation valve with another PRV help the situation? This would allow two pressure drops across two valves from 1600 to 400 psi.
Also, does steam cut valves when they are cycled or condesate or both?
Thanks for the input.