what alloy contains 64% Ni and 30% Cu thanks
 
Where is the other 6% for a mass of 100%? This could be Monel.
 
Must be a variation of Monel 400.
63-70% Ni, up to 5% Fe+Si+Mn (they each have limits), bal Cu

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 