Dec 18, 2012 #1 Nileshjp Materials Dec 18, 2012 1 0 0 US Is Ozone being produced during corona treatment of PET films?
Dec 18, 2012 #2 Demon3 Materials Jun 6, 2005 1,850 0 0 US I have done some work on that. Ozone can be produced in some cases. I found ozone when using silicone electrodes on PVC. When we used ceramic electrodes we didn't find any. All the best, Chris Chris DeArmitt - PhD FRSC CChem Plastic & Additives Webinars Instant Downloads & Inexpensive http://www.plastictraining.com Upvote 0 Downvote
I have done some work on that. Ozone can be produced in some cases. I found ozone when using silicone electrodes on PVC. When we used ceramic electrodes we didn't find any. All the best, Chris Chris DeArmitt - PhD FRSC CChem Plastic & Additives Webinars Instant Downloads & Inexpensive http://www.plastictraining.com
Dec 18, 2012 #3 Demon3 Materials Jun 6, 2005 1,850 0 0 US Looks like there's an ozone test available for $80 US. I made one for $3. Hoping to commercialize it one day. Chris DeArmitt - PhD FRSC CChem Plastic & Additives Webinars Instant Downloads & Inexpensive http://www.plastictraining.com Upvote 0 Downvote
Looks like there's an ozone test available for $80 US. I made one for $3. Hoping to commercialize it one day. Chris DeArmitt - PhD FRSC CChem Plastic & Additives Webinars Instant Downloads & Inexpensive http://www.plastictraining.com
Dec 18, 2012 #4 Compositepro Chemical Oct 22, 2003 7,721 0 36 US Corona treatment does create ozone and nitrogen oxides, which are toxic and also have a fairly strong and distinct odor. Upvote 0 Downvote
Corona treatment does create ozone and nitrogen oxides, which are toxic and also have a fairly strong and distinct odor.