Jtgevoc

Chemical
Dec 21, 2013
2
Thinking of building a large evaporator to concentrate salt solutions to 25% +/-.
Planning to use 2205 tubing and contact surfaces. Vapor surfaces will be 316L

Any experience?

Thanks Jtgevoc

 
Replies continue below

Recommended for you

None that worked. If it is absolutely deaerated and it is cold then it might work.
I can't see 316 working if any liquid contacts it at all.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Thanks Ed,
Probably run seven effects forward flow evaporator, single pass.
If my first effect is at 100 degree C at 3% salt, will the 2205 work?
(I assume this will be the most severe condition).

The last effect will be at about 50 degrees C and 25% concentration.

I can build the entire evaporator out of 2205