What are the recommended corrosion preventive methods for 9% Nickel steel LNG tanks during filling for and during hydrotest with an anticipated maximum exposure time of 60 days? Do We Have any Corrosion in fresh water in this Test?
 
Replies continue below

Recommended for you

I would recommend a corrosion inhibitor if you intend to keep water in the vessels for 60 days. Fresh water means nothing to me other than risk of corrosion - bio, oxygen, chlorides, etc.
 
We used a film forming, biodegradable, corrosion inhibitor from Cortec.
 