Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Corrosion rated of uncoated steel

Status
Not open for further replies.

71corvette

Structural
Feb 26, 2003
105
Can anyone provide generally accepted anticipated rates of corrosion for uncoated steel exposed to the elements? I realize the rates of corrosion will vary based on a myriad of environmental criteria, but are there some basic ranges of corrosion rates that can be provided?

Thanks,
Tim
 
Replies continue below

Recommended for you

In a typical environment corrosion rates have been determined at: 0.008in/yr.

In more corrosive environments rates extend to 0.012in/yr.

You can find this information in many FHWA or NCHRP references.