Hi everybody,
Do you know where to find a reliable database of time dependent (10000h, 100000h, 200000h) creep rupture strength values for SA387 Gr.11 Cl.1.
In the EN 10028-2 some EU mat properties are given but I have no information about ASTM materials.
I would very much appreciate a good tip.
 
Replies continue below

Recommended for you

I recall some published data circa 1978 in the asme journal of mechanics (?), creep testing of low alloys related to the clinch river breeder reactor with related creep life curves. In general, those bound papers are nomally first published at the ASME PVP conference, so you may check the asme archives .
 