Hi Everbody,
I came across and noted NACE MR0175/ISO 15156-2 Table A.2 considered API 5L pipes up to grade X65 material as prequalified material for SSC resistance complying with A.2.1 requirements.
May we extend that to CSA Z245.1 Steel Line pipe up to Gr. 448 which has similar Yield strength and same criteria for fabrication as X65 to be prequalified?
Is there any NACE interpretation allowing that?
Thanks!
I came across and noted NACE MR0175/ISO 15156-2 Table A.2 considered API 5L pipes up to grade X65 material as prequalified material for SSC resistance complying with A.2.1 requirements.
May we extend that to CSA Z245.1 Steel Line pipe up to Gr. 448 which has similar Yield strength and same criteria for fabrication as X65 to be prequalified?
Is there any NACE interpretation allowing that?
Thanks!