Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

curve fitting 100% compressible ogden foam

Status
Not open for further replies.

Malmskov

Mechanical
Joined
Feb 8, 2010
Messages
4
Location
DK
hi
I'm trying to model a highly compressible material in ansys via curve fitting. I have the test Strain/stress data for uniaxial compression. As I'm assuming the material will only deform in one direction I have set my uniaxial test data in tbft,eadd as seen below

0 0 0
0.357142857 0 0.100
0.448979592 0 0.176
0.517857143 0 0.264
0.571428571 0 0.342
0.614285714 0 0.424
0.649350649 0 0.520
0.678571429 0 0.615

where the first coloumb is Engineering Strain
the 2'd is Lateral Direction Engineering Strain
and the 3'd Engineering Strain

Because of 100% compressio im fixing b=0.
When putting pressure on top af the material and trying to solve it ANSYS terminates the analysis after a while with the following:
reason for termination........error in element formulation.
And when im checking the last step the deformation is much higher compared to the data I've used
Does anyone know why this happens or have an idea what I'm doing wrong?

Thank You
 
Malmskov,

I'm sorry that I don't have an answer for you. However, I'd suggest you post this question to the ANSYS forum of Eng-Tips, as it seems to deal primarily with the ANSYS code and not necessarily the mechanics of the problem. Good luck

Peter
 