Hi all,

We sent some brass components, CZ121, out to be stress relieved at 260 degree. The purchasing department unfortunately "copy and pasted" the information incorrectly. The parts have been annealed by taking them to 650 degrees and air cooled.

Is there anyway of recovering these components to the condition originally specified?

Thanks

Dom
 