Background:
The code in question is AWS D1.1:2015. There have been no exceptions or deviations of any sort granted by the EOR.
This is a production weldment, using a combination of listed and unlisted materials.
The weld shop will be using several pre-qualified GMAW WPS’s. They will also be using GMAW WPS’s qualified by PQR, as well as GMAW-S WPS’s qualified by PQR, all for a variety of listed and unlisted materials.
The weld shop contracts with a local AWS-CWI to help with their testing, paperwork and so forth.
My function is to review the weld shops documents and decide if they meet the contract specifications, and can be made part of the permanent quality records for the actual parts.
Situation:
When reviewing the PQR’s, at this point I have only looked at the PQR’s for GMAW-S, I am looking at the portion that I feel is dealt with in Clause 4.9, Methods of Testing and Acceptance Criteria.
I see the VT portion signed off on. I see values listed in the tensile pull portion. I see information about the bend tests. What I don’t see is anything in relation to the RT/UT portion, except that the CWI who completed the form has filled those blanks in with “NA”.
When I look at the code book, I see in the first paragraph under 4.9, it says “the welded test assemblies conforming to 4.9.2…”. 4.9.2 states that before preparing any mechanical test specimens, the test plate SHALL be non-destructively tested using RT or UT, and the requirements for those are spelled out in 4.9.2.1
When asked about it, the CWI who signed and stamped the completed form states “It is my professional interpretation that AWS D1.1 does not require a nondestructive (RT/UT) testing procedure to qualify a GMAW-S PQR”.
Finally, we get to the actual questions:
Which person is correct?
I am not interpreting, I am strictly going by what it says in black and white, it says RT/UT SHALL be performed. The CWI is interpreting. What is he interpreting, how does he arrive at it, what allows him to interpret, and what am I missing if he is correct?
Many thanks in advance!
The code in question is AWS D1.1:2015. There have been no exceptions or deviations of any sort granted by the EOR.
This is a production weldment, using a combination of listed and unlisted materials.
The weld shop will be using several pre-qualified GMAW WPS’s. They will also be using GMAW WPS’s qualified by PQR, as well as GMAW-S WPS’s qualified by PQR, all for a variety of listed and unlisted materials.
The weld shop contracts with a local AWS-CWI to help with their testing, paperwork and so forth.
My function is to review the weld shops documents and decide if they meet the contract specifications, and can be made part of the permanent quality records for the actual parts.
Situation:
When reviewing the PQR’s, at this point I have only looked at the PQR’s for GMAW-S, I am looking at the portion that I feel is dealt with in Clause 4.9, Methods of Testing and Acceptance Criteria.
I see the VT portion signed off on. I see values listed in the tensile pull portion. I see information about the bend tests. What I don’t see is anything in relation to the RT/UT portion, except that the CWI who completed the form has filled those blanks in with “NA”.
When I look at the code book, I see in the first paragraph under 4.9, it says “the welded test assemblies conforming to 4.9.2…”. 4.9.2 states that before preparing any mechanical test specimens, the test plate SHALL be non-destructively tested using RT or UT, and the requirements for those are spelled out in 4.9.2.1
When asked about it, the CWI who signed and stamped the completed form states “It is my professional interpretation that AWS D1.1 does not require a nondestructive (RT/UT) testing procedure to qualify a GMAW-S PQR”.
Finally, we get to the actual questions:
Which person is correct?
I am not interpreting, I am strictly going by what it says in black and white, it says RT/UT SHALL be performed. The CWI is interpreting. What is he interpreting, how does he arrive at it, what allows him to interpret, and what am I missing if he is correct?
Many thanks in advance!