da storage vessel weld cracks

Status
Not open for further replies.

bhart192

Civil/Environmental
Feb 6, 2006
81
Looking into weld cracking on DA storage vessels ,seems that PWHT is recommended ,also grinding weld reinforcement flush, I can follow PWHT but not flush weld cap . any thoughts are appreciated
 
Replies continue below

Recommended for you

Why can't you blend grind the weld caps of a repair weld or flush patch plate? I would strongly recommend PWHT AND blend grind the repair welds to eliminate stress risers.
 
Fun with Dearerators..... An ongoing discussion..!!!

Damn, there have been certainly some good, informed people on these hallowed fora.




Tell us more about your DA details....sizes, pressures etc

Is this a new or existing unit ?

Are you brave
 